PofoliaGünlük literatür takibi

Polymer Bulletin· 2026Q2

Poli(viniliden florür) ve epoksitlenmiş doğal kauçuk karışımlarında faz-morfoloji evrimi ve baryum titanatın belirgin tercihli lokalizasyonu ile ayarlanabilir mekanik ve dielektrik özellikler

Phase-morphology evolution and apparent preferential localization of barium titanate in poly(vinylidene fluoride) and epoxidized natural rubber blends with tunable mechanical and dielectric properties

Subhan Salaeh, Philippe Cassagnau, Charoen Nakason

Kısa özet

Baryum titanat (BT), poli(viniliden florür) (PVDF)/ENR-50 karışımlarında epoksitlenmiş doğal kauçuğa (ENR-50) tercihli olarak ayrışarak, 80/20 karışımındaki ENR-50 alanlarının ortalama boyutunu 6.5'ten 11.4 µm'ye çıkarır ve PVDF sürekliliğini değiştirmez.

Yapay zekâ ile başlık ve abstract'tan üretildi; tam metin okunmaz.

Ana noktalar

  • Baryum titanat (BT) parçacıkları, PVDF/ENR-50 karışımlarında epoksitlenmiş doğal kauçuk (ENR-50) fazına tercihli olarak ayrışır.
  • BT eklenmesi, 80/20'lik bir karışımda ENR-50 alanlarının ortalama boyutunu 6.5'ten 11.4 µm'ye çıkarırken PVDF sürekliliğini değiştirmedi.
  • Faz inversiyonu, PVDF'den ENR-50 sürekliliğine geçiş yaparak 60/40 ve 20/80 PVDF/ENR-50 kompozisyonları arasında gerçekleşti.
  • ENR-50 içeriğinin artması sertliği ve çekme gerilimini azaltırken, kopma uzaması %1000-2200'e varan değerlerle uzayabilirliği önemli ölçüde artırdı.

Yapay zekâ ile başlık ve abstract'tan üretildi; tam metin okunmaz.

Özet (abstract)

Abstract Non-vulcanized blends of poly(vinylidene fluoride) (PVDF) with epoxidized natural rubber containing 50 mol% epoxide (ENR-50) in 80/20–20/80 wt% ratios were prepared by melt blending. The PVDF/ENR-50 blends at 80/20 and 50/50 were filled with 5 vol% barium titanate (BT). SEM analysis revealed a change in morphology from PVDF continuity to apparent co-continuity at 60/40–50/50, followed by ENR-50 continuity at higher ENR-50 content. Increasing the ENR-50 content reduced stiffness and tensile stress but increased extensibility, with elongation at break values of about 1000–2200% in the ENR-50-rich blends. Furthermore, the PVDF crystallization temperature increased from 135.8°C in neat PVDF to 139.3°C at the 50/50 composition, whereas normalized PVDF crystallinity decreased from 54.2% at 60/40 to 43.7% at 20/80 due to phase confinement. Relaxation peaks at − 36 and − 9°C indicated phase separation with partial interface compatibility. The novelty lies in the identification of two-phase inversion boundaries and the correlation between phase continuity and mechanical, thermal, dynamic-mechanical, and dielectric behavior. Moreover, BT particles preferentially segregated to ENR-50, increasing the average size of ENR-50 domains in the 80/20 blend from 6.5 to 11.4 µm without altering PVDF continuity.

Yazarların özeti; kaynağından alınmıştır. Polymer Bulletin, 2026 · DOI ↗

ÇıkarımlarPremium Makaleye SorÜcretsiz hesapla

Ücretsiz hesapla devam et

Makaleye Sor ile bu makaleye günde 5 soru ücretsiz; makaleyi kaydet, kaynakçasını al, ilgi alanına göre her gün yeni özetler. Çıkarımlar Premium.

Web'de ücretsiz devam et

Google ya da Apple hesabınla giriş; kart istemez. Bu makaleye geri dönersin.

Telefonda:

Alan: Polimerler ve Plastikler

Polymers and PlasticsMaterials Science