BMC Oral Health· 2026Q1
Multi-indicator finite element analysis of the mechanical response of NiTi orthodontic archwires with titanium nitride coatings of varying thickness
- 0citations
- Q1SCImago
- 2026year
Short summary
Finite element analysis reveals that Titanium Nitride (TiN) coatings between 800–1300 nm on NiTi orthodontic archwires yield optimal stiffness, load-bearing capacity, and cyclic stability, with smaller diameter wires showing greater performance gains.
AI-generated from the title and abstract; the full text is not read.
Key points
- TiN coatings enhance stiffness, load-bearing capacity, and cyclic stability of NiTi archwires.
- An optimal TiN coating thickness range of 800–1300 nm yields the most balanced mechanical performance.
- Coating thicknesses beyond this range lead to saturation of strengthening effects and potential stress concentrations.
- Smaller diameter archwires exhibit higher performance gains from TiN coatings.
- The study analyzed parameters like von Mises stress, elastic strain energy density, and axial displacement.
AI-generated from the title and abstract; the full text is not read.
Abstract
Abstract To enhance the mechanical stability and resistance to plastic damage of Nickel-Titanium (NiTi) orthodontic archwires, this study employs numerical simulations to investigate the multiscale mechanical responses of three types of archwires with different diameters (0.014, 0.016, and 0.018 inch) coated with Titanium Nitride (TiN) of varying thicknesses (550–1550 nm) under uniaxial tension and cyclic loading. The study focuses on analyzing key parameters such as von Mises stress, elastic strain energy density, equivalent deviatoric strain, and axial displacement, and it explores the regulation mechanisms of TiN thickness variation in stiffness enhancement, stress sharing, energy storage, and deformation suppression. The results indicate that the TiN coating can enhance the overall stiffness, load-bearing capacity, and cyclic stability of the archwires; reduce plastic strain accumulation; and optimize energy distribution, among which the thickness range of 800–1300 nm yields the most balanced overall performance. When the coating thickness exceeds the critical value, the strengthening effect tends to saturate, and adverse boundary effects such as a local stress concentration may occur. In addition, archwires with smaller diameters are more sensitive to coating reinforcement, exhibiting higher performance gains. This study reveals the multiscale regulation mechanisms governing the mechanical properties of NiTi archwires as a function of TiN coating thickness, providing a theoretical basis and design guidance for their structural optimization and surface engineering.
The authors' abstract, as published at the source. BMC Oral Health, 2026 · DOI ↗
Continue with a free account
Ask the paper: 3 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.
Continue free on the webSign in with Google or Apple; no card needed. You come back to this paper.
On your phone:
Field: Orthodontics
OrthodonticsDentistry