Phosphate-treated siwak as a calcium phosphate–bearing bioactive material for fluoride-free oral care: physicochemical characterization and in vitro enamel microhardness recovery

Amine Yerou, Mohamed Elmeguenni, B. Bachir Bouiadjra, Abdulmohsen Albedah

Short summary

A novel fluoride-free toothpaste formulation using phosphate-treated siwak (Salvadora persica) effectively recovered enamel microhardness by 137% (from 127.93 ± 5.93 HV to 300.19 ± 5.08 HV) after 7 days, matching the performance of hydroxyapatite.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Phosphate treatment of siwak powder created a calcium and phosphate-bearing material.
  • Fluoride-free toothpastes were formulated with either phosphate-treated siwak or hydroxyapatite.
  • Enamel microhardness recovered from 127.93 ± 5.93 HV (demineralized) to 300.19 ± 5.08 HV with phosphate-treated siwak.
  • The recovery achieved by phosphate-treated siwak was statistically similar to that of hydroxyapatite (p = 0.863).

AI-generated from the title and abstract; the full text is not read.

Abstract

Phosphate-treated siwak ( Salvadora persica ) was developed as a calcium phosphate-bearing bioactive material and evaluated for its in vitro enamel remineralization potential when incorporated into a fluoride-free toothpaste. Siwak powder was phosphate-treated with phosphoric acid under controlled conditions and characterized by X-ray fluorescence (XRF), scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM/EDS), Fourier transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD). Fluoride-free laboratory toothpastes were formulated with phosphate-treated siwak or hydroxyapatite (HAp) as the active material. Twenty independent bovine teeth were allocated to four groups ( n = 5 per group). Surface Vickers microhardness was evaluated at the tooth level, with five indentations averaged per specimen, and analyzed using Welch’s one-way ANOVA followed by Games–Howell pairwise comparisons. Phosphate treatment produced Ca/P-bearing signatures by XRF/EDS together with phosphate-associated FTIR and XRD features. Mean surface microhardness was 265.93 ± 2.12 HV in sound enamel, 127.93 ± 5.93 HV in the post-demineralization reference group, 300.19 ± 5.08 HV after the 7-day phosphate-treated siwak protocol, and 295.25 ± 13.31 HV after the HAp protocol. Overall group differences were significant (Welch ANOVA: F(3, 7.71) = 813.21, p < 0.0001), while no statistically significant difference was detected between the two treatment groups ( p = 0.863). Enamel FTIR showed qualitative condition-associated differences in phosphate-region features. These findings support preliminary proof-of-concept evidence that phosphate-treated siwak can participate in a treatment protocol associated with enamel surface microhardness recovery. Because the post-demineralization reference was measured immediately whereas the treated groups underwent an additional 7-day period in artificial saliva, the microhardness comparisons represent the net effect of the complete treatment protocol rather than the isolated effect of the active toothpaste component.

The authors' abstract, as published at the source. Scientific Reports, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: General Dentistry

General DentistryDentistry