PofoliaDaily literature tracker

Coatings· 2026Q2

Effect of Deposition Defects on the Wear and Corrosion Resistance Behavior of HVOF-Sprayed 304 Stainless Steel Coatings

Ting Zhang, Wensheng Li, Haimin Zhai, Xinjian Zhang et al.

Short summary

The OF-4.7/D-250 HVOF-sprayed 304 stainless steel coating, with 1.8% porosity and 2.1% oxygen, achieved the lowest wear rate of (1.60 ± 0.01) × 10−5 mm3·N−1·m−1 and corrosion current density of (1.29 ± 0.09) × 10−6 A·cm−2, demonstrating that deposition defects significantly impact these properties.

AI-generated from the title and abstract; the full text is not read.

Key points

  • HVOF spraying parameters influence particle melting, spreading, and solidification, affecting coating porosity, oxide content, and phase composition.
  • The OF-4.7/D-250 coating showed the densest structure with 1.8 vol. % porosity and 2.1 wt. % oxygen.
  • This optimal coating achieved the lowest wear rate of (1.60 ± 0.01) × 10−5 mm3·N−1·m−1 and corrosion current density of (1.29 ± 0.09) × 10−6 A·cm−2.
  • Wear resistance is influenced by porosity, oxides, and phase composition, while corrosion resistance is mainly affected by porosity and oxides.
  • Deposition defects are identified as the dominant factor controlling wear and corrosion resistance in these coatings.

AI-generated from the title and abstract; the full text is not read.

Abstract

In this study, 304 stainless steel (304SS) coatings were deposited by high-velocity oxygen-fuel (HVOF) spraying at varying oxygen-fuel (OF) ratios and spraying distances. The effects of deposition defects and solidification phase structures on dry sliding wear and electrochemical corrosion were systematically investigated. The results indicate that the spraying parameters altered particle melting, spreading, solidification, and oxidation, thereby governing porosity, oxide content, and phase composition of the coatings. Consequently, the OF-4.7/D-250 coating exhibited the densest structure, with 1.8 vol. % porosity, 2.1 wt. % oxygen, and approximately 10 wt. % martensite, achieving the lowest wear rate of (1.60 ± 0.01) × 10−5 mm3·N−1·m−1 and corrosion current density (1.29 ± 0.09) × 10−6 A·cm−2. Wear resistance is collectively influenced by porosity, oxides, and phase composition, whereas corrosion resistance is mainly affected by porosity, followed by oxides. Austenite remained dominant in all coatings (≥77 wt. %), so the influence of phase composition on corrosion was comparatively limited. The deposition defects dominate the variation in wear and corrosion resistance of the HVOF-sprayed 304SS coatings.

The authors' abstract, as published at the source. Coatings, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Surfaces, Coatings and Films

Surfaces, Coatings and FilmsMaterials Science