PofoliaDaily literature tracker

Scientific Reports· 2026Q1

Layer-specific effects of an ultra-speed sintering protocol on translucency and microstructure of yttria-gradient zirconia

Hye-Jeong Shin, Mi-Hyang Cho, Hyo‐Joung Seol

Short summary

Ultra-speed (US) sintering reversed the translucency relationship between incisal and cervical layers of yttria-gradient zirconia, significantly reducing incisal translucency beyond acceptability thresholds while increasing residual pores and grain size.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Ultra-speed (US) sintering reversed the translucency hierarchy between incisal and cervical layers of yttria-gradient zirconia.
  • Incisal layer translucency decreased significantly (Δ TP 00 : 2.78–3.00) after US sintering, surpassing the acceptability threshold.
  • US sintering increased residual pores and grain size in the incisal layer, from 1.13–1.14 µm to 2.94–2.98 µm.
  • Phase composition shifted with an increased yttria-rich t′-phase and decreased t-phase fraction after US sintering.

AI-generated from the title and abstract; the full text is not read.

Abstract

Abstract This study evaluated the effects of ultra-speed (US) sintering on the translucency and microstructure of yttria-gradient zirconia. Eighty specimens were prepared from two yttria-gradient zirconias (5 mol% yttria-stabilized incisal and 4 mol% yttria-stabilized cervical layers). Each layer underwent conventional (CS) or US sintering. Translucency ( TP 00 ) was measured spectrophotometrically (n = 10/group). Microstructure, grain size, and phase composition were analyzed using field-emission scanning electron microscopy (n = 4/group) and Rietveld refinement (n = 2/group). Translucency was analyzed using three-way ANOVA, and grain size using a generalized linear model (α = 0.05). Under CS, the incisal layer ( TP 00 : 8.01–8.12) was more translucent than the cervical layer (7.27–7.45), whereas this relationship was reversed after US sintering. This reversal reflected a significant reduction in TP 00 in the incisal layer (Δ TP 00 : 2.78–3.00), exceeding the translucency acceptability threshold, while cervical changes remained within the translucency perceptibility threshold. Residual pores were more evident in the incisal layer after US sintering, with grain size increasing from 1.13–1.14 to 2.94–2.98 µm. After US sintering, the yttria-rich t′ -phase fraction increased, whereas the t -phase fraction decreased in both layers. These findings provide further insight into the potential layer-specific response of yttria-gradient zirconias to US sintering.

The authors' abstract, as published at the source. Scientific Reports, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: General Dentistry

General DentistryDentistry