PofoliaDaily literature tracker

Sustainability· 2026Q1

Management of Chemical Processes in the Production of Thermal Insulation Materials to Improve Water Resistance and Environmental Safety

Roman Dychkovskyi, Artem Pavlychenko, Dariusz Sala, Michał Pyzalski et al.

Short summary

A new thermal insulation composite (composition no. 1) achieved a water susceptibility of 2.1% by optimizing the water-to-cement ratio to 0.55 and gas-forming powder content to 0.14 g, while maintaining low material cost (EUR 0.120/kg).

AI-generated from the title and abstract; the full text is not read.

Key points

  • Optimized thermal insulation composite (composition no. 1) achieved 2.1% water susceptibility.
  • Water susceptibility ranged from 2.1% to 6.8% across ten experimental formulations.
  • Lowest water susceptibility was linked to a W/C ratio of 0.55 and 0.14 g gas-forming powder.
  • Composition no. 1 also had the lowest estimated material cost at EUR 0.120/kg.
  • Coordinated control of W/C ratio, pore-forming component, and polymer modifiers is crucial for material performance.

AI-generated from the title and abstract; the full text is not read.

Abstract

Thermal insulation materials play a crucial role in improving the energy efficiency and durability of buildings; however, their long-term performance can be significantly affected by moisture exposure. This study investigates the relationship between the formulation parameters, water susceptibility, structural stability, environmental performance, and economic efficiency of lightweight thermal insulation composites. Ten experimental formulations were produced by systematically varying the cement content, water-to-cement ratio (W/C), gas-forming powder content, and polymer-modifying additives. Water resistance was evaluated through controlled immersion tests and measurements of mass variation and structural condition, supported by response-surface analysis. The experimentally determined water susceptibility ranged from 2.1% to 6.8%, demonstrating a systematic increase with increasing W/C ratio and gas-forming powder content. The most favorable result was obtained for composition no. 1, characterized by a W/C ratio of 0.55 and a powder content of 0.14 g, which exhibited the lowest water susceptibility of 2.1%. In our previous studies, the developed waste-based thermal insulation materials demonstrated a density of up to 550 kg/m3 and thermal conductivity below 0.12 W/(m·K). Building on these results, the present study focuses on their water absorption and water-resistance characteristics. Composition No. 1 also showed the lowest estimated material cost, approximately EUR 0.120/kg (EUR 66.04/m3), demonstrating that improved moisture resistance can be achieved without compromising economic efficiency. The results establish a quantitative composition–structure–property relationship and demonstrate that coordinated control of the W/C ratio, pore-forming component, and polymer modifiers is essential for balancing moisture resistance, thermal performance, material cost, and environmental sustainability. The proposed integrated assessment framework supports the development and selection of durable thermal insulation composites for sustainable construction, while further long-term durability, leaching, and life-cycle assessments are required to confirm their environmental performance under realistic service conditions.

The authors' abstract, as published at the source. Sustainability, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Building and Construction

Building and ConstructionEngineering