PofoliaDaily literature tracker

Journal of Prosthodontic Research· 2026Q1

Comparison of the mechanical and bonding properties of vat photopolymerization resin and resin composite blocks

Jiaxu Chen, Ryuhei Kanda, Susumu Tsuda, Yoshiya Hashimoto et al.

Short summary

Vat photopolymerization (VPP)-fabricated definitive crown material (Sprintray Ceramic Crown) showed significantly lower flexural strength (~50-60%) and Vickers hardness (~30-40%) compared to conventional CAD-CAM hybrid composite resin (HCR) blocks (Shofu Block HC Hard II and Cerasmart Prime), and exhibited greater wear loss.

AI-generated from the title and abstract; the full text is not read.

Key points

  • VPP-fabricated Sprintray Ceramic Crown had 50-60% of the flexural strength of CAD-CAM HCR blocks.
  • VPP material exhibited 30-40% of the Vickers hardness compared to CAD-CAM HCR blocks.
  • The VPP material showed greater wear loss than conventional CAD-CAM HCR materials.
  • All tested materials achieved clinically acceptable shear bond strengths, exceeding 15 MPa.

AI-generated from the title and abstract; the full text is not read.

Abstract

PURPOSE: This study compared the mechanical properties, wear behavior, and shear bond strength (SBS) of resin luting agents in additive-manufactured composite crown materials intended for definitive restorations with those of conventional computer-aided design/computer-aided manufacturing (CAD-CAM) hybrid composite resin (HCR) block materials. METHODS: Sprintray Ceramic Crown (SP) was used as the representative vat photopolymerization (VPP)-fabricated material based on additive manufacturing, whereas Shofu Block HC Hard II (HC) and Cerasmart Prime (CS) were selected as CAD-CAM HCR block materials. The mechanical properties were evaluated using three-point flexural strength and Vickers hardness tests. The wear behavior was examined via a reciprocating sliding test using an alumina ball antagonist. The SBS was measured between each material and various resin-luting agents. RESULTS: SP showed ~50-60% of the flexural strength and 30-40% of the Vickers hardness of HC and CS. Wear testing revealed that SP exhibited greater wear loss than those of CAD-CAM HCRs. The SBS values of SP with each resin cement were slightly lower than those of HC and CS under most conditions; however, all values exceeded 15 MPa, indicating a clinically acceptable bond strength. CONCLUSIONS: The VPP-fabricated definitive crown material (SP) demonstrated inferior mechanical properties and wear resistance compared to those of conventional CAD-CAM HCRs. However, the acceptable levels of bond strength were observed, highlighting the importance of careful case selection for definitive restorations.

The authors' abstract, as published at the source. Journal of Prosthodontic Research, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: General Dentistry

General DentistryDentistry