Potassium Sorbate-Modified Adhesive Layers in Greaseproof Cardboard Inserts: Mechanical Performance, Migration Behaviour and Technological Validation

Marcin Cichosz, Joanna Wyrwas, Mieczysława Katarzyna Nath, Urszula Kiełkowska

Short summary

Potassium sorbate-modified adhesives in greaseproof cardboard inserts demonstrated the lowest overall migration (3.61 ± 0.38 mg·dm−2 at 4.0% w/w) among tested modifiers, while maintaining a normalised breaking force of 144.2–181.6 N·m−1.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Potassium sorbate-modified adhesives showed the lowest overall migration (3.61 ± 0.38 mg·dm−2) compared to sodium alginate and chitosan at 4.0% (w/w).
  • Normalised breaking force for potassium sorbate formulations ranged from 144.2–181.6 N·m−1.
  • A preliminary technological window for potassium sorbate was found to be 4.30–4.55% (w/w).
  • Higher adhesive dosage (15 g·m−2 vs. 9 g·m−2) significantly increased migration.
  • The 4.90% potassium sorbate formulation exceeded migration limits and reduced breaking force.

AI-generated from the title and abstract; the full text is not read.

Abstract

Paper- and cardboard-based food-contact materials require solutions that combine mechanical integrity, controlled migration and technological simplicity. This study evaluated greaseproof cardboard inserts in which the aqueous adhesive layer was modified with sodium alginate, chitosan or potassium sorbate. Initial formulation screening comprised eight concentrations (0.5–4.0% (w/w)) for each modifier, with ten adhesive-joint strength measurements per formulation (240 measurements in total). Overall migration to modified polyphenylene oxide (MPPO; Tenax®) was determined at an additive concentration of 4.0% (w/w), using ten measurements per modifier. Further experiments evaluated adhesive application side, adhesive dosage (9 and 15 g·m−2), creasing intensity (0–20 crease lines), and potassium sorbate concentrations of 4.30, 4.55 and 4.90% (w/w). Among the tested modifiers, potassium sorbate combined relatively high mechanical performance with lower overall migration: normalised breaking force remained within 144.2–181.6 N·m−1 across the initial screening range, and overall migration at 4.0% (w/w) was the lowest among the three modifiers (3.61 ± 0.38 mg·dm−2). Additional migration validation yielded 4.678 ± 0.292 and 4.779 ± 0.158 mg·dm−2 for the 4.30 and 4.55% formulations, respectively, whereas the 4.90% formulation showed substantially higher migration (8.737 ± 0.204 mg·dm−2) and reduced breaking force below the internal technological acceptance criterion. Increasing adhesive dosage from 9 to 15 g·m−2 significantly increased migration within both investigated exposure protocols. The 4.30–4.55% (w/w) potassium sorbate range was identified as a preliminary technological window under the investigated conditions. Given the limited number of independent production batches and the absence of formal statistical optimisation, this interval should not be interpreted as a statistically established optimum or a generalisable formulation limit. Antimicrobial efficacy and shelf-life extension were not investigated.

The authors' abstract, as published at the source. Technologies, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Biomaterials

BiomaterialsMaterials Science