Journal of Vacuum Science & Technology A Vacuum Surfaces and Films· 2026Q2
Crystallinity evolution of metal–organic chemical vapor deposition -grown β-Ga2O3 heteroepitaxial films probed by high-temperature x-ray diffraction under different reactor heights
- 1citations
- Q2SCImago
- 2026year
Short summary
Metal-organic chemical vapor deposition (MOCVD) reactor height significantly impacts the crystallinity and structural response of β-Ga2O3 films at elevated temperatures, with shorter chambers yielding smoother films and distinct thermal expansion behavior compared to longer chambers.
AI-generated from the title and abstract; the full text is not read.
Key points
- Reactor height in MOCVD influences the initial crystallinity and morphology of β-Ga2O3 films.
- Shorter MOCVD chambers produced β-Ga2O3 films with smoother surfaces (RMS roughness 7.3 nm vs. 12.3 nm after heating).
- β-Ga2O3 films from shorter chambers showed a more reversible lattice expansion response during high-temperature XRD (25-1100 °C).
- Rocking curve FWHM evolution differed significantly between films grown in short and long chambers, indicating distinct structural responses to heat.
AI-generated from the title and abstract; the full text is not read.
Abstract
The crystallinity of β-Ga2O3 thin films grown by metal–organic chemical vapor deposition (MOCVD) is strongly influenced by reactor design. We investigate the effect of reactor height on crystallinity in MOCVD-grown β-Ga2O3 films by directly comparing long- and short-chamber showerhead configurations. The β-Ga2O3 films were grown heteroepitaxially on c-plane α-Al2O3 (0001) substrates with the (−201) orientation for 40 min at a growth rate of approximately 1 μm/h. Structural evolution was probed by high-temperature x-ray diffraction (HT-XRD) during heating from 25 to 1100 °C. Temperature-dependent XRD reveals a systematic red shift of the β-Ga2O3 (−201) reflection toward lower 2θ upon heating for both reactor geometries, followed by a blue shift toward the initial position upon cooling, consistent with a largely reversible, thermally driven lattice-expansion response. Temperature-dependent rocking-curve analysis reveals distinct FWHM evolution for the two films: the short-chamber film decreases from approximately 2.83° at 25 °C to ∼2.65° at 500 °C before broadening to ∼2.85° at 1100 °C, whereas the long-chamber film broadens from approximately 2.07° to ∼2.38° over the same temperature range; after cooling, the respective FWHM values recover to approximately 2.72° and 2.03°. Atomic force microscopy shows smoother short-chamber films, with root-mean-square roughness decreasing from 7.7 to 7.3 nm after HT-XRD heating, compared with 19.3–12.3 nm for long-chamber films. Overall, these results indicate that reactor height influences the initial crystalline and morphological templates of β-Ga2O3 films and modulates their elevated-temperature structural response, providing practical insights into optimizing MOCVD reactor design for high-quality β-Ga2O3 growth.
The authors' abstract, as published at the source. Journal of Vacuum Science & Technology A Vacuum Surfaces and Films, 2026 · DOI ↗
Continue with a free account
Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.
Continue free on the webSign in with Google or Apple; no card needed. You come back to this paper.
On your phone:
Field: Electronic, Optical and Magnetic Materials
Electronic, Optical and Magnetic MaterialsMaterials Science