PofoliaDaily literature tracker

Polymer Bulletin· 2026Q2

Phase-morphology evolution and apparent preferential localization of barium titanate in poly(vinylidene fluoride) and epoxidized natural rubber blends with tunable mechanical and dielectric properties

Subhan Salaeh, Philippe Cassagnau, Charoen Nakason

Short summary

Barium titanate (BT) preferentially segregates to epoxidized natural rubber (ENR-50) in poly(vinylidene fluoride) (PVDF)/ENR-50 blends, increasing ENR-50 domain size from 6.5 to 11.4 µm in an 80/20 blend, without altering PVDF continuity.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Barium titanate (BT) particles preferentially segregate to the epoxidized natural rubber (ENR-50) phase in PVDF/ENR-50 blends.
  • BT addition increased ENR-50 domain size from 6.5 to 11.4 µm in an 80/20 blend, without altering PVDF continuity.
  • Phase inversion occurred between 60/40 and 20/80 PVDF/ENR-50 compositions, transitioning from PVDF to ENR-50 continuity.
  • Increasing ENR-50 content reduced stiffness and tensile stress but significantly increased extensibility, with elongations at break reaching 1000–2200%.

AI-generated from the title and abstract; the full text is not read.

Abstract

Abstract Non-vulcanized blends of poly(vinylidene fluoride) (PVDF) with epoxidized natural rubber containing 50 mol% epoxide (ENR-50) in 80/20–20/80 wt% ratios were prepared by melt blending. The PVDF/ENR-50 blends at 80/20 and 50/50 were filled with 5 vol% barium titanate (BT). SEM analysis revealed a change in morphology from PVDF continuity to apparent co-continuity at 60/40–50/50, followed by ENR-50 continuity at higher ENR-50 content. Increasing the ENR-50 content reduced stiffness and tensile stress but increased extensibility, with elongation at break values of about 1000–2200% in the ENR-50-rich blends. Furthermore, the PVDF crystallization temperature increased from 135.8°C in neat PVDF to 139.3°C at the 50/50 composition, whereas normalized PVDF crystallinity decreased from 54.2% at 60/40 to 43.7% at 20/80 due to phase confinement. Relaxation peaks at − 36 and − 9°C indicated phase separation with partial interface compatibility. The novelty lies in the identification of two-phase inversion boundaries and the correlation between phase continuity and mechanical, thermal, dynamic-mechanical, and dielectric behavior. Moreover, BT particles preferentially segregated to ENR-50, increasing the average size of ENR-50 domains in the 80/20 blend from 6.5 to 11.4 µm without altering PVDF continuity.

The authors' abstract, as published at the source. Polymer Bulletin, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Polymers and Plastics

Polymers and PlasticsMaterials Science