Coupled degradation and mechanical performance of additively manufactured poly(L-lactic acid) esophageal stents: Influence of strut thickness

Saeed Sanjari, Shahram Etemadi Haghighi, Payam Saraeian, Ali Alinia-ziazi

Short summary

Additively manufactured PLLA esophageal stents with thinner struts (0.8 mm) offer greater initial flexibility but fail mechanically by day 52, while thicker struts (1.6 mm) retain structural integrity longer, despite lower initial compliance.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Both 0.8 mm and 1.6 mm PLLA stent designs experienced a ~90% reduction in molecular weight over 90 days in accelerated degradation tests.
  • Thinner (0.8 mm) stents provided higher initial flexibility but failed mechanically by day 52.
  • Thicker (1.6 mm) stents maintained structural integrity longer, despite lower initial compliance.
  • Load-bearing capacity correlated with molecular weight, while radial stiffness correlated with crystallinity.

AI-generated from the title and abstract; the full text is not read.

Abstract

Achieving predictable degradation for bioresorbable esophageal stents remains a significant challenge. The influence of strut thickness (0.8 and 1.6 mm) on the coupled chemical degradation and mechanical stability of additively manufactured poly (L-lactic acid) (PLLA) esophageal stents is investigated via accelerated in vitro degradation (50°C, 90 days). Molecular weight, crystallinity, thermal transitions, and mechanical properties are assessed via gel permeation chromatography, differential scanning calorimetry, and mechanical testing (three-point bending and radial compression). Molecular weight decreases by approximately 90% over 90 days, with a similar half-life (t 1 / 2 ≈ 25 days) for both thicknesses, indicating bulk-dominated hydrolysis and autocatalytic degradation. At the number-average molecular weight (M n) half-life, both designs show substantial reductions in flexural and radial performance; however, crystallinity evolution and mechanical loss are strongly thickness-dependent. Thinner stents provide greater initial flexibility but undergo rapid embrittlement and mechanical failure by day 52, whereas thicker designs retain structural integrity longer despite lower initial compliance. Correlation analysis reveals that load-bearing capacity strongly correlates with M n, while radial stiffness associates with crystallinity. Consequently, strut thickness is a critical design parameter governing the degradation-performance profile of additively manufactured PLLA stents. These findings quantify the trade-off between initial flexibility and long-term stability, informing the optimization of bioresorbable, patient-specific esophageal stents.

The authors' abstract, as published at the source. Journal of Thermoplastic Composite Materials, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Biomaterials

BiomaterialsMaterials Science