PofoliaShared via Pofolia

Trends in Applied Sciences Research· 2012

Structural Characterization of Selected Indian Coals by X-ray Diffraction and Spectroscopic Techniques

B. Manoj, A. G. Kunjomana

Short summary

Indian coals contain turbostratic crystalline carbon and amorphous carbon, with crystallite sizes (La, Lc) and interlayer spacing (d002) indicating lower order than pure graphite.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Indian coals comprise turbostratic crystalline carbon and amorphous carbon.
  • Crystallite lateral sizes (La) range from 28.15-38.43 A°, stacking heights (Lc) from 22.64-20.16 A°, and interlayer spacing (d002) from 3.52-3.34 A°.
  • These structural parameters indicate a lower degree of crystalline order compared to pure graphite.
  • Spectroscopic analysis confirmed graphite layer formation and the presence of aromatic and aliphatic functional groups.
  • Coal structural parameters correlate strongly with elemental carbon and volatile content, reflecting coal rank.

AI-generated from the title and abstract; the full text is not read.

Abstract

The structural parameters of three Indian coals were determined by X-ray diffraction, Raman, UV-Vis-NIR, FTIR spectroscopy and SEM-EDS. This study reveals that the coals contain crystalline carbon of turbo- stratic structure with some amount of amorphous carbon. The average lateral sizes (La), stacking heights (Lc) and interlayer spacing (d002) of the crystallite structures calculated from the X-ray intensities range from 28.15-38.43 A°, 22.64-20.16A° and 3.52-3.34 A°, respectively which is higher than that of pure graphite, suggesting a low degree of crystalline order in the studied sample. The decrease in La with rank shows that the carbon in coal is nano crystalline in structure. Raman spectroscopic study confirms the presence of multi layer formation of graphite layer. The defect band at 1355 cm-1 is due to benzene or condensed benzene rings present in amorphous carbon. The FTIR spectra of the coals show the presence of stretching vibrations of -OH bonds, aliphatic -CH, -CH2 and -CH3 absorptions, C = C and -CH of aromatic structure. The C-H bending frequencies have higher intensity than the C-H stretching band. This is due to the intense broad absorption produced in this region by graphite components. A strong linear relationship exists between the coal structural parameters (fa,d002,Lc) and the elemental carbon and volatile contents of the coal which reflects the dependency of the coals structure on their ranks. The SEM image shows the presence of layered structure on the surface. The EDS analysis confirms the presence of Carbon and Oxygen on the surface. The absorption maximum of benzene-oxygen system was found between 235-270 nm. The weak band at the 680 nm is attributed to the ∏-∏* electronic transitions of the polynuclear aromatic hydrocarbons.

The authors' abstract, as published at the source. Trends in Applied Sciences Research, 2012 · DOI ↗

TakeawaysPremium
Ask the paperFree account

Continue with a free account

Ask the paper: 3 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Fuel Technology

Fuel TechnologyEnergy