European Journal of Wood and Wood Products· 2026Q2
Influence of the internal air temperature on properties of wood-plastic composites processed by rotational molding
- 0citations
- Q2SCImago
- 2026year
Short summary
A peak internal air temperature (PIAT) of 208°C ensures optimal properties and prevents thermal degradation in rotomolded wood-plastic composites (WPC) made of 85% recycled HDPE and 15% capirona wood particles.
AI-generated from the title and abstract; the full text is not read.
Key points
- A peak internal air temperature (PIAT) of 208°C is optimal for rotomolded WPC (85% recycled HDPE, 15% capirona wood), preventing degradation and ensuring good properties.
- Pure recycled HDPE requires a PIAT of 233°C for full densification.
- The six phases of the rotational molding process can be identified by analyzing the second derivative of internal air temperature profiles.
AI-generated from the title and abstract; the full text is not read.
Abstract
In the processing of wood-plastic composites ( WPC ) by rotational molding, thermal decomposition of wood can occur due to the high temperatures of the process. However, it can be avoided by controlling the peak internal air temperature ( PIAT ). In this perspective, the main purpose of this work is to determine how the PIAT and the properties of the rotomolded WPC are related to each other. To achieve this, several materials were processed using different oven temperatures and heating times. As a consequence, the PIAT reached a specific value during the process in each case. Then, characterization tests were carried out to determine mechanical and physical properties of the obtained materials. Finally, using the test results, a relationship between the PIAT and those properties was defined. The rotomolded WPC were made of 85% of recycled high-density polyethylene ( HDPER ) and 15% of capirona wood particles ( CWP ), but materials made of 100% of HDPER were also processed. Results show that a PIAT of 208 °C is required for a rotomolded WPC to be fully densified. Under this condition, it has optimal properties and it does not undergo thermal degradation. As for the material made of 100% of HDPER , a PIAT of 233 °C is necessary to reach such state. In addition, using the second derivative of the internal air temperature profiles, the beginning and end of the six phases of the rotational molding process were identified, too.
The authors' abstract, as published at the source. European Journal of Wood and Wood Products, 2026 · DOI ↗
Continue with a free account
Ask the paper: 3 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.
Continue free on the webSign in with Google or Apple; no card needed. You come back to this paper.
On your phone:
Field: Polymers and Plastics
Polymers and PlasticsMaterials Science