PofoliaDaily literature tracker

Metals· 2026Q2

Effect of Annealing Time on Microstructure Evolution and Mechanical Properties of Hot-Rolled Cu–Zn–Sn Alloy

Longfei Zhai, Shuangli Lu, Lei Li, Huan Yan et al.

Short summary

Annealing a hot-rolled Cu–Zn–Sn alloy at 500 °C for 5 hours yields optimal strength and ductility, achieving 451.6 MPa UTS and 41.7% elongation by controlling recrystallization, phase transformation, and Sn-rich intergranular phase formation.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Annealing at 500 °C for 5 hours yields optimal strength-ductility synergy in hot-rolled Cu–Zn–Sn alloy.
  • Optimal conditions achieve 451.6 MPa ultimate tensile strength and 41.7% elongation.
  • Annealing time controls recrystallization, phase transformation, and Sn-rich intergranular phase content.
  • The Sn-rich intergranular phase acts as a damage source, while solid-solution and dislocation strengthening are key.
  • Fracture mode transitions from ductile dimples to mixed ductile-brittle based on Sn-rich phase distribution.

AI-generated from the title and abstract; the full text is not read.

Abstract

The effect of post-rolling annealing time on the microstructural evolution and room-temperature mechanical properties of a hot-rolled Cu–Zn–Sn alloy was systematically investigated. The alloy was isothermally annealed at 500 °C for 4, 5, and 6 h. Results reveal that annealing time non-monotonically governs the recrystallization of the α and β phases and the final content of the Sn-rich intergranular phase, coupled with the α/β phase transformation and Sn partitioning. The as-hot-rolled microstructure comprises a dual α + β structure without the Sn-rich intergranular phase. After 4 h, the α phase recrystallizes completely, and the β phase fraction decreases, leading to Sn rejection and Sn-rich intergranular phase formation after furnace cooling; hardness and strength are minimum, while ductility is high. At 5 h, the β phase fraction recovers and Sn partitions into the β phase, decreasing the final Sn-rich intergranular phase content. The β phase transforms into fine short-rod and lath-like morphologies, refining grains and yielding optimal strength–ductility synergy, with an ultimate tensile strength (UTS) of 451.6 MPa and an elongation of 41.7%. At 6 h, the β phase fraction decreases and grains coarsen, leading to re-formation of the Sn-rich intergranular phase and degraded strength. Quantitative analysis reveals that solid-solution strengthening provides a stable baseline, while variations in yield strength are dominated by dislocation and grain-boundary strengthening. The β phase provides load-transfer strengthening, and the Sn-rich intergranular phase acts primarily as a damage source. Fracture changes from ductile dimples to mixed ductile–brittle with local flat features, depending on the Sn-rich intergranular phase distribution. This study links processing, microstructure, and properties for optimizing tin brass heat treatment.

The authors' abstract, as published at the source. Metals, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

General Materials ScienceMaterials Science