Hydrogen charging in ultrafine-grained medium-Mn steel caused a rate-dependent ductility loss, with relative elongation decreasing from 24% at a strain rate of 1.7×10−3 s−1 to 48% at 1.7×10−4 s−1.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Hydrogen charging caused a pronounced, rate-dependent loss of ductility in ultrafine-grained medium-Mn steel.
  • Relative elongation loss increased from 24% at a strain rate of 1.7×10−3 s−1 to 48% at 1.7×10−4 s−1.
  • Lower strain rates intensified hydrogen-assisted damage accumulation without altering the primary damage sites.
  • Damage was preferentially associated with ferrite grain/subgrain boundaries, ferrite/austenite interfaces, and DIM regions.

AI-generated from the title and abstract; the full text is not read.

Abstract

The strain-rate dependence of hydrogen-assisted damage evolution was investigated in an ultrafine-grained Fe–6Mn–2Al–1Si–0.4C medium-Mn steel using tensile testing, interrupted microstructural characterization, subsurface microscopy, and fractography. Hydrogen charging caused pronounced rate-dependent ductility loss, with relative elongation loss increasing from 24% at 1.7×10−3 s −1 to 48% at 1.7×10−4 s −1 , while the uncharged specimens showed closely comparable tensile responses. Interrupted microstructural characterization revealed similar retained-austenite fractions at both strain rates, while the lower strain rate produced greater local misorientation in both the ferrite-dominated and austenitic constituents. Hydrogen-assisted damage was preferentially associated with ferrite grain/subgrain boundaries, ferrite/austenite and ferrite/DIM interfaces, DIM regions, and cementite-related interfaces. These preferred sites remained similar at both rates, but damage features were more frequent at the lower rate. Fracture remained predominantly dimpled, with localized ferrite/cementite interfacial separation. Thus, decreasing strain rate primarily intensified hydrogen-assisted damage accumulation rather than changing DIM extent and preferred damage sites.

The authors' abstract, as published at the source. International Journal of Hydrogen Energy, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Metals and Alloys

Metals and AlloysMaterials Science