Faraday Discussions· 2027Q1
Electrocatalytic performance enhancement through coalescence-induced bubble dynamics: the case of the anode
- 2citations
- Q1SCImago
- 2027year
Short summary
Coalescence of oxygen bubbles on an anode surface can trigger earlier detachment, reducing anodic overpotential by up to 200 mV and doubling reaction current under specific conditions.
AI-generated from the title and abstract; the full text is not read.
Key points
- Bubble coalescence can induce earlier oxygen bubble detachment from the anode, improving electrochemical performance.
- Anodic overpotential was reduced by up to 200 mV, and reaction current increased by a factor of ≈2 due to coalescence-induced detachment.
- Earlier bubble departure enables stable operation at higher currents that would otherwise be limited by electrode blockage.
- Coalescence becomes inhibited at current densities above ≈1 mA, leading to larger detachment sizes.
AI-generated from the title and abstract; the full text is not read.
Abstract
Electrolytically generated hydrogen and oxygen bubbles can substantially reduce the efficiency of (water) electrolysis by blocking the active electrode area and increasing ohmic losses. There is therefore an interest in strategies to improve bubble removal, particularly under microgravity where buoyancy, which favors bubble departure under terrestrial conditions, is absent. Both in alkaline and acidic electrolytes, O2 bubbles tend to remain at the electrode for longer, in part due to solutal Marangoni effects, and detach at significantly larger sizes compared to H2 bubbles. As an alternative to buoyancy-driven removal, coalescence between a pair of bubbles can induce bubble detachment from the electrode and is therefore a highly attractive mechanism. Building on our previous work demonstrating that coalescence-induced H2 bubble departure can enhance electrochemical performance using a dual Pt microelectrode system, we now extend this approach to the oxygen evolution reaction in HClO4, KOH and H2SO4. By combining high-speed imaging with electrochemical measurements, we show that coalescence can trigger substantially earlier O2 bubble departure as compared to buoyancy effects alone, reducing the anodic overpotential by up to ∼100-200 mV under galvanostatic conditions, which is equivalent to an enhancement of the reaction current by up to a factor of ≈2 under potentiostatic conditions. Earlier bubble departure also enables stable operation at substantially higher currents that would otherwise be limited by the bubbles blocking the electrode surface. At elevated currents, however, we find that coalescence between neighbouring bubbles becomes progressively inhibited and delayed, leading to larger detachment size and eventually preventing the formation of a single bubble beyond ≈1 mA. Finally, in contrast to previous observations for H2 in H2SO4, our data shows that once departed, O2 bubbles are unlikely to return to the electrode via repeated near-electrode coalescence. We attribute this contrast between O2 and H2 bubbles to the inherently lower O2 gas production rate, which is half that of H2 at a fixed current.
The authors' abstract, as published at the source. Faraday Discussions, 2027 · DOI ↗
Continue with a free account
Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.
Continue free on the webSign in with Google or Apple; no card needed. You come back to this paper.
On your phone:
Field: Renewable Energy, Sustainability and the Environment
Renewable Energy, Sustainability and the EnvironmentEnergy