ACS Catalysis· 2012Q1
Electrocatalytic Oxygen Evolution Reaction (OER) on Ru, Ir, and Pt Catalysts: A Comparative Study of Nanoparticles and Bulk Materials
- 2,561citations
- Q1SCImago
- 2012year
Short summary
Ru and Pt nanoparticles show significantly worse OER performance and durability than their bulk counterparts, while Ir nanoparticles offer comparable activity and durability to bulk Ir, suggesting Ir nanoparticles are promising for OER.
AI-generated from the title and abstract; the full text is not read.
Key points
- Ru nanoparticles suffer from strong corrosion and cannot sustain OER, unlike bulk Ru.
- Pt nanoparticles show lower initial OER activity and deactivate during stability tests, unlike bulk Pt.
- Ir nanoparticles exhibit OER activity and durability comparable to bulk Ir.
- Nanoscaling has the most pronounced negative effects on Ru and Pt OER performance and durability.
AI-generated from the title and abstract; the full text is not read.
Abstract
A comparative investigation was performed to examine the intrinsic catalytic activity and durability of carbon supported Ru, Ir, and Pt nanoparticles and corresponding bulk materials for the electrocatalytic oxygen evolution reaction (OER). The electrochemical surface characteristics of nanoparticles and bulk materials were studied by surface-sensitive cyclic voltammetry. Although basically similar voltammetric features were observed for nanoparticles and bulk materials of each metal, some differences were uncovered highlighting the changes in oxidation chemistry. On the basis of the electrochemical results, we demonstrated that Ru nanoparticles show lower passivation potentials compared to bulk Ru material. Ir nanoparticles completely lost their voltammetric metallic features during the voltage cycling, in contrast to the corresponding bulk material. Finally, Pt nanoparticles show an increased oxophilic nature compared to bulk Pt. With regard to the OER performance, the most pronounced effects of nanoscaling were identified for Ru and Pt catalysts. In particular, the Ru nanoparticles suffered from strong corrosion at applied OER potentials and were therefore unable to sustain the OER. The Pt nanoparticles exhibited a lower OER activity from the beginning on and were completely deactivated during the applied OER stability protocol, in contrast to the corresponding bulk Pt catalyst. We highlight that the OER activity and durability were comparable for Ir nanoparticles and bulk materials. Thus, Ir nanoparticles provide a high potential as nanoscaled OER catalyst.
The authors' abstract, as published at the source. ACS Catalysis, 2012 · DOI ↗
Continue with a free account
Ask the paper: 3 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.
Continue free on the webSign in with Google or Apple; no card needed. You come back to this paper.
On your phone:
Field: Renewable Energy, Sustainability and the Environment
Renewable Energy, Sustainability and the EnvironmentEnergy