Scientific Reports· 2026Q1

Achieving resistivity and thermal stability balance in Cu‑xMn‑3Ni-based alloy resistors for smart energy meters

Tao Hu, Wenlong Liu, Yu Meng, Zhi Li et al.

Short summary

A Cu-17Mn-3Ni alloy quenched at 750°C and aged at 260°C achieves a balanced resistivity of 0.46 μΩ m and a low TCR of 29 ppm/°C, making it suitable for high-stability precision resistors in smart energy meters.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Increasing Mn content in Cu-xMn-3Ni alloys strengthens (311) plane orientation, increasing resistivity and decreasing TCR.
  • The dominant texture factor in Cu-17Mn-3Ni alloy shifts from thermodynamic stability to kinetic resistance with rising quenching temperature.
  • A specific heat treatment (quenching at 750°C, aging at 260°C) eliminates residual stresses.
  • The optimized alloy exhibits a resistivity of 0.46 μΩ m and a TCR of 29 ppm/°C.

AI-generated from the title and abstract; the full text is not read.

Abstract

High-stability precision resistance alloys are core functional components for DC shunts and high-end smart energy meters. The synergistic control of low resistivity and low temperature coefficient of resistance (TCR) is critical for their service performance under high power conditions. Cu‑Mn‑Ni‑based alloys offer a balanced combination of electrical conductivity and thermal stability, and alloying and heat treatment are the key technical approaches for optimizing their properties. In this work, the effects of Mn content and quenching process on the microstructure, electrical resistivity and TCR of hot‑rolled Cu‑ x Mn‑3Ni-based alloys were investigated. With increasing Mn content, the preferential orientation of the (311) plane becomes stronger, while that of the (111) crystal plane weakens, and the resistivity increases whereas the TCR decreases. As the quenching temperature rises from 500 to 800 °C, the dominant factor governing texture in the Cu-17Mn-3Ni-based alloy evolution changes from internal‑stress‑driven thermodynamic stability to kinetic resistance of grain boundary migration, and the (220) plane becomes the dominant preferred orientation. After quenching at 750 °C followed by aging at 260 °C, the effective elimination of residual stresses enables the alloy to possess both appropriate electrical resistivity (0.46 μΩ m) and excellent thermal stability (TCR = 29 ppm/°C). This work highlights that the composition synergistic heat treatment provides a feasible strategy to develop precision resistance alloys with balanced resistivity and temperature stability.

The authors' abstract, as published at the source. Scientific Reports, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

General Materials ScienceMaterials Science