Short summary

Boric anhydride and sodium polyphosphate accelerate phase transformation in silica-based dry ramming mixes, with boric anhydride being more suitable for silica from Hubei and Hebei, while Henan-derived silica requires a high content (3 wt%) of sodium polyphosphate for optimal properties at 1550 °C.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Boric anhydride and sodium polyphosphate accelerate phase transformation in silica-based dry ramming mixes.
  • Fine-grained, high-purity quartz from Hubei exhibits the fastest phase formation at 1550 °C.
  • Sodium polyphosphate induces significant volumetric expansion at 1400 °C, which diminishes with increased concentration at 1550 °C.
  • Boric anhydride is more effective for silica from Hubei and Hebei.
  • Henan-derived silica requires 3 wt% sodium polyphosphate for optimal properties at 1550 °C.

AI-generated from the title and abstract; the full text is not read.

Abstract

This study systematically investigated how sintering aid type and amount, silica properties, and temperature affect the characteristics of silica-based dry ramming mixes. We selected boric anhydride and sodium polyphosphate as the sintering aids. Phase evolution results and properties evaluated via X-ray diffraction analysis and property testing indicate that fine-grained, high-purity quartz from Hubei presented the fastest phase formation after firing at 1550 °C. Both sintering aids accelerated phase transformation; however, additional boric anhydride did not modify the process further. Sodium polyphosphate caused pronounced volumetric expansion of up to 20% at 1400 °C, but this expansion gradually decreased as sodium polyphosphate increased at 1550 °C. The sintering behavior and properties of silica-based dry ramming mixes were governed by the interplay between the extent of phase transformation (dominant at 1400 °C) and the quantity of liquid phase (dominant at 1550 °C). Overall, boric anhydride is more suitable for silica from Hubei and Hebei; however, based on the conditions assessed in the present investigation, a high content of sodium polyphosphate (3 wt%) is required for Henan-derived silica.

The authors' abstract, as published at the source. Applied Sciences, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Ceramics and Composites

Ceramics and CompositesMaterials Science