Virtual and Physical Prototyping· 2026Q1

Fiber-orientation controlled C f /SiC composites with anisotropic thermal conductivity via additive manufacturing and reactive melt infiltration

Huisheng Tian, Yang Xia, Buhao ZHANG, Jiayi Geng et al.

Short summary

Researchers fabricated Cf/SiC composites with controlled fiber alignment and anisotropic thermal conductivity (1.5 ratio) using a combination of additive manufacturing and reactive melt infiltration, achieving a thermal conductivity of 130.1 W·m−1·K−1 along the preferred direction.

AI-generated from the title and abstract; the full text is not read.

Key points

  • Cf/SiC composites with controlled fiber orientation were fabricated using additive manufacturing and reactive melt infiltration.
  • Roller-induced shear forces during laser printing aligned carbon fibers in-plane.
  • A protective layer around fibers mitigated reactions with molten silicon during infiltration.
  • The composites achieved a fiber orientation factor of 0.7789 and a thermal conductivity of 130.1 W·m−1·K−1 along the preferred direction.
  • A thermal anisotropy ratio of 1.5 was observed, demonstrating direction-dependent thermal transport.

AI-generated from the title and abstract; the full text is not read.

Abstract

Manipulation of fiber alignment provides an effective means of tailoring the directional thermal transport properties of Cf/SiC composites. However, maintaining the designed fiber orientation during subsequent high-temperature densification remains challenging, particularly during silicon infiltration, where molten Si can strongly react with Cf. Here, fiber-orientation-controlled Cf/SiC composites were fabricated by combining selective laser printing, polymer infiltration and pyrolysis processing, and reactive melt infiltration. During laser printing, roller-induced shear forces promoted the in-plane alignment of high aspect ratio Cf, establishing a preferential fiber orientation within the printed body. Subsequent infiltration and pyrolysis of polycarbosilane and phenolic resin formed a protective layer around the fibers, mitigating their reaction with molten Si. The resulting composites exhibited a fiber orientation factor of 0.7789 and a bulk density of 2.87 ± 0.04 g·cm−3, with a flexural strength of 268.1 ± 15.3 MPa along the preferred direction. The preserved fiber orientation led to direction-dependent thermal transport, with a thermal conductivity of 130.1 W·m−1·K−1 along the preferred direction and a thermal anisotropy ratio of 1.5. These results demonstrate that combining additive manufacturing with interfacial protection and RMI provides an effective strategy for preserving designed fiber alignments while achieving highly densified Cf/SiC composites with anisotropic thermal transport.

The authors' abstract, as published at the source. Virtual and Physical Prototyping, 2026 · DOI ↗

TakeawaysPremium Ask the paperFree account

Continue with a free account

Ask the paper: 5 free questions a day about this paper; save it, get its citation, new summaries every day for your field. Takeaways are Premium.

Continue free on the web

Sign in with Google or Apple; no card needed. You come back to this paper.

On your phone:

Field: Ceramics and Composites

Ceramics and CompositesMaterials Science